Electrical Properties Metric English Comments
Comparative Tracking Index 370 V

@Temperature 23.0 °C
370 V

@Temperature 73.4 °F
IEC 60112
DuPont Performance Polymers Crastin® SK615SF NC010 PBT  (Unverified Data**)
Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc..