Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 375 V | 375 V | IEC 112 |
Qualchem Danamid AFGF-15 Polyamide 66, 15% Glass Fiber Reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 112 |
Qualchem Danamid AFGF-20 Polyamide 66, 20% Glass Fiber Reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 112 |
Qualchem Danamid AFGF-30 Polyamide 66, 30% Glass Fiber Reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Comparative Tracking Index | 375 V | 375 V | |
Polimeri Europa EDISTIR N1841 Polystyrene
(discontinued **) Symbol according to ISO 1043-1: PS Designation: Thermoplastic ISO 1622-PS,M,085-12 General purpose polystyrene combining easy flow and medium heat. This grade exhibits excellent processability in .. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
Lanxess Durethan® BKV 15 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, good heat-ageing resistance |
|||
Comparative Tracking Index | >= 375 V | >= 375 V | IEC 60112 |
SABIC Innovative Plastics LNP THERMOCOMP PF005 PA 6 (Europe-Africa-Middle East) 25% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Comparative Tracking Index | 375 V | 375 V | Solution A; IEC 60112 |
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph.. |
|||
Comparative Tracking Index | 375 V | 375 V | GB/4207 |
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6 Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
Polyplastics Duranex® 3300 Polybutylene Terephthalate (PBT), Standard, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Comparative Tracking Index | 375 V | 375 V | M; IEC 60112 |
Eurostar Staramide AG7H PA66, 35% Glass Filled, Injection Molded AG7 is a Heat Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 375 V | 375 V | M; IEC 60112 |
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 375 V | 375 V | M; IEC 60112 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Comparative Tracking Index | 375 V | 375 V | M; IEC 60112 |
Eurostar Staramide BG6U PA6, 30% Glass Fiber Filled, UV Stabilized, Injection Molded Staramide BG6U is an UV Stabilized, 30% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 375 V | 375 V | M; IEC 60112 |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 375 V | 375 V | M; IEC 60112 |
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 60112 |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Comparative Tracking Index | 375 V | 375 V | |
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Comparative Tracking Index | 375 V | 375 V | |
BASF Polystyrol® 165 H Polystyrene (Europe) High molecular grades, often blended with high-impact extrusion grades (e.g. for dairy products).Data was collected by ISO methods and provided by BASF. |
|||
Comparative Tracking Index | 375 V | 375 V | |
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe) Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Comparative Tracking Index | 375 V | 375 V | Test Solution A; IEC 60112 |
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation.. |
|||
Comparative Tracking Index | 375 V | 375 V | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Comparative Tracking Index | 375 V | 375 V | IEC 112 |
LATI LASTIROL TR G/10-V1 10% Glass Fiber Reinforced Polystyrene (PS) (UL94 V-1)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Comparative Tracking Index | 375 V | 375 V | Test solution A; IEC 60112 |
BASF Ultradur B 4300 G6 30% Glass Filled PBT Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Comparative Tracking Index | 375 V | 375 V | Test Solution A; IEC 60112 |
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT Description: Easy flowing injection molding grade with 30 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg windshield wiper arms, printed circuit boards PCBs), housing, .. |