Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 125 - 550 V | 125 - 550 V | Average value: 337 V Grade Count:12 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |