Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 85.0 - 400 V | 85.0 - 400 V | Average value: 237 V Grade Count:12 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |