Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.025 ohm | 0.025 ohm | |
Lord Adhesives Metech 3504 Palladium Silver Conductor Composition Designed for use in the manufacture of hybrid circuitry, resistor networks, potentiometers as well as general purpose microcircuitry. It employs a conventional glass bonding mechanism, has wide proc.. |
|||
Surface Resistivity per Square | <= 0.025 ohm | <= 0.025 ohm | 100 square pattern cured at 150ºC for 5 minutes |
Lord Adhesives Metech 6103 Silver Conductor This material is a low viscosity thermoplastic printing ink designed for general purpose application onto various rigid substrate compositions such as epoxy board or other rigid plastic. It is desig.. |
|||
Surface Resistivity per Square | <= 0.025 ohm @Thickness 0.0250 mm |
<= 0.025 ohm @Thickness 0.000984 in |
|
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |