Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 0.10 - 100 ohm | 0.10 - 100 ohm | |
Nanosonic Metal Rubber™ Metal Rubber™ is a unique self-assembled nanocomposite material that combines the high electrical conductivity of metals with the low mechanical modulus of elastomers. Self-assembly processing allo.. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | [ohm/in<sup>2<sup>]; <.016 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FAB CRS Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | |
Parker Chomerics CHO-SHIELD® 2003 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | CEPS-0002 |
Parker Chomerics SOFT-SHIELD® 5000 Low Closure Force EMI Gasket Description: SOFT-SHIELD® 5000 Series EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electron.. |
|||
Surface Resistivity per Square | >= 0.10 ohm | >= 0.10 ohm | |
Parker Chomerics WIN-SHIELD™ Mesh 100 EMI Shielding Mesh Blackened copper plating. WIN-SHIELD Mesh 100 provides exceptional shielding performance and can be used as an optical product, to cover airflow openings, to wrap cable or other applications where .. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | [ohm/in<sup>2<sup>]; <.016 ohm/cm<sup>2</sup>; MIL-STD-202C |
Parker Chomerics CHO-FAB CFT Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | cured |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | |
Parker Chomerics CHO-SHIELD® 2001 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Surface Resistivity per Square | <= 0.10 ohm | <= 0.10 ohm | |
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |