Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® HDPE - High Density Polyethylene (ASTM Product Data Sheet) Natural and Black |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® PP, Natural Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Sanalite® HDPE - High Density Polyethylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Surface Resistivity per Square | 1.00e+15 - 1.00e+16 ohm | 1.00e+15 - 1.00e+16 ohm | ASTM D257 |
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | ASTM D-257 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Wanshijie PC Film PC is a kind of shapeless, odorless, non-toxic, high transparency, colorless or light yellow thermoplastic engineering plastic with excellent physical and mechanical properties, especially excellent.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
Westlake Plastics MediPEEK T Polyetheretherketone for Medical Applications MediPEEK-T is a high performance semi-crystalline thermoplastic designed for short term body contact as an implantable material. It is USP Class VI and ASTM F2026 compliant. It has excellent steri.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 10 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 418 Paper, 14 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Dry; ASTM D257 |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 23.0 °C |
1.00e+15 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT™ 2021 Polyimide, Brown (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 500 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 92 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 400 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm @Temperature 25.0 °C |
1.00e+15 ohm @Temperature 77.0 °F |
500 V DC @ 50% RH; ASTM D257 |
DuPont Teijin Films Melinex® S Polyester Film, 48 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Non-adhesive side; ASTM D257 |
3M 4104 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Adhesive side; ASTM D257 |
3M 4104 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | 1.00e+15 ohm | 1.00e+15 ohm | Adhesive side; ASTM D257 |
3M 4108 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet) |
|||
Surface Resistivity per Square | >= 1.00e+15 ohm | >= 1.00e+15 ohm | VDE 0303 |
GEHR Plastics PPE Polyphenylene Ether
(discontinued **) Polyphenylenether belongs to the group of amorphous materials and can be used in temperatures ranging from -50°C to approximately 105°C. PPE exhibits a high impact strength, a low water absorption.. |