Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | <= 1.0e+7 ohm | <= 1.0e+7 ohm | IEC 60093 |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |