Polymer Property : Surface Resistivity per Square = 18 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 10 - 18 ohm
10 - 18 ohm
Coating
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating
Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst..
Surface Resistivity per Square 10 - 18 ohm
10 - 18 ohm
Parker Chomerics Tecknit Teckfilm™ Transparent Conductive Coating on Polyester Film
Description: TECKFILM is a highly conductive coating deposited on a transparent polyester film. It is available in rolls 30" wide. Usable width is 28". The conductive coating is overcoated with a ce..