Electrical Properties Metric English Comments
Surface Resistivity per Square 2.30e+13 ohm
2.30e+13 ohm
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..