Polymer Property : Surface Resistivity per Square = 6.10e+10 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistivity per Square 6.10e+10 ohm
6.10e+10 ohm
CTM E042
Nanocyl PLASTICYL™ PP2001 Polypropylene with 2 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..