Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 6.20e+15 ohm | 6.20e+15 ohm | GB/T1410-2006 |
Sichuan Deyang Haton® hMR60DL Polyphenylene Sulfide, Glass & Mineral Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |