Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | 9.10e+13 ohm | 9.10e+13 ohm | |
Saint-Gobain Korel® K30-15 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Surface Resistivity per Square | 9.10e+13 ohm | 9.10e+13 ohm | |
Saint-Gobain Korel® K30-20 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |
|||
Surface Resistivity per Square | 9.10e+13 ohm | 9.10e+13 ohm | |
Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |