Electrical Properties Metric English Comments
Surface Resistivity per Square 31 - 95 ohm

@Thickness 0.0250 mm
31 - 95 ohm

@Thickness 0.000984 in
Printed through 230 stainless steel mesh with 13 micron emulsion
Gwent Electronic Materials C2100126D6 Carbon Graphite Ink
This ink is designed for biosensor applications, it gives a good electrochemical response when tested with buffered Ferricyanide solutions. This product is based on a unique curing process that resu..