Arc Resistance 104 sec
104 sec
ASTM D495
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **)
Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat..
Arc Resistance 104 sec
104 sec
ASTM D495
Toyobo TS401 PPS, 40% Glass Fiber Reinforced
Key Feature: General Purpose Grade - balanced characteristics suitable for a broad range of uses.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a spec..
Arc Resistance 104 sec
104 sec
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant
BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was..