Electrical Properties Metric English Comments
Arc Resistance 126 sec
126 sec
ASTM D495
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Arc Resistance 126 sec
126 sec
ASTM D495
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy
EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc.
Arc Resistance 126 sec
126 sec
ASTM D495
Plenco 2535 Phenolic, Granular, Injection Molded
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c..
Arc Resistance 126 sec
126 sec
ASTM D495
Toyobo Vylopet® EMC415 PET/PBT Blend
Key Feature: HB UL-94 ClassApplications: accessory componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high di..
Arc Resistance 126 sec
126 sec
Dow Corning 7 RELEASE COMPOUND
Silicone-based compound, light consistencyInformation provided by Dow Corning
Arc Resistance 126 sec
126 sec
IPC TM-650 2.5.1
Arlon GenClad™ 280 Low Loss Thermoset Bond-Ply
Low loss Ceramic-Filled Thermoset/Thermoplastic Hybrid SystemRivals PTFE laminate electrical performance in a Halogen-Free systemLight weight material relative to standard laminate materialsOptimal ..