Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 139 sec | 139 sec | ASTM D495 |
Glastic Laminates/Shapes FHT Flexible High Temperature Polyester Laminate Data provided by Glastic Corporation.Excellent flexibility plus good electrical strength retention values after long term heat aging. Widely used in motors and dry type transformers. |
|||
Arc Resistance | 139 sec | 139 sec | UL recognition value, tungsten electrode; ASTM D495 |
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Arc Resistance | 139 sec | 139 sec | ASTM D495 |
Ascend Performance Materials VYDYNE® R220 Nylon, Mineral Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |