Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 77.0 - 146 sec | 77.0 - 146 sec | Average value: 121 sec Grade Count:3 |
Overview of materials for Phenolic, Novolac, Impact Grade, Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Impact Grade, Filled". Each property range of values reported is minimum and maximum .. |