Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 146 sec | 146 sec | ASTM D495 |
Plenco 7697 Phenolic, Granular, Compression Molded PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform.. |