Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 120 - 200 sec | 120 - 200 sec | Average value: 175 sec Grade Count:8 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Arc Resistance | 180 - 200 sec | 180 - 200 sec | ASTM D495-61 |
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther.. |