Electrical Properties Metric English Comments
Arc Resistance 320 sec
320 sec
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Compression Moldings
Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn..
Arc Resistance 320 sec
320 sec
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings
Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn..