Electrical Properties Metric English Comments
Arc Resistance 370 sec
370 sec
Pyrotek NAD-11 Structural Insulation Board
NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation ..
Arc Resistance 370 sec
370 sec
Pyrotek NAD-500 Electrical Insulation Product
Cement reinforcement, Inorganic fiber resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasket..