Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 67 sec | 67 sec | ASTM D495 |
LG Chemical Lupox® PBT-GP-2306F 30% GFR Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Arc Resistance | 67 sec | 67 sec | ASTM D495 |
Plenco 7487 Phenolic, Granular, Transfer Molded PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple.. |