Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Arc Resistance = 87.0 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Arc Resistance 87.0 - 183 sec
87.0 - 183 sec
Average value: 144 sec Grade Count:9
Overview of materials for Phenolic, Resole, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of ..
Arc Resistance 87.0 - 129 sec
87.0 - 129 sec
Average value: 107 sec Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..
Copyright © lookpolymers.com All Rights Reserved