Electrical Properties Metric English Comments
Arc Resistance 93 sec
93 sec
Practical Use (Water Absorption 1.25%); ASTM-D495
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..