Polymer Property : Static Decay = 0.050 sec
Polymer Property :
Static Decay =
0.050 sec
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Static Decay
0.050
sec
0.050
sec
Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled
Conductive Carbon, Powder Modified