Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 1.3 sec | 1.3 sec | 12% RH (+5000 V to 50 V); FTMS-101C |
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy sys.. |
|||
Static Decay | 1.3 sec | 1.3 sec | 12% RH (-5000 V to -50 V); FTMS-101C |
Lubrizol STAT-RITE® E-1150 Ether-Type Static Dissipative Polymer Description: IStat-Rite® E-1150 blend is a static dissipative thermoplastic polyurethane (TPU) alloy. Stat-Rite E-1150 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy sys.. |