Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | <= 2.0 sec | <= 2.0 sec | MIL PFR-81705D |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Static Decay | <= 2.0 sec | <= 2.0 sec | MIL PFR-81705D |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |