Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | -23.0 dB @Thickness 1.57 mm, Frequency 8.00e+9 Hz |
-23.0 dB @Thickness 0.0620 in, Frequency 8.00e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Shielding Effectiveness | -23.0 dB @Thickness 1.57 mm, Frequency 8.00e+9 Hz |
-23.0 dB @Thickness 0.0620 in, Frequency 8.00e+9 Hz |
Microwave Absorption |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |