Polymer Property : Shielding Effectiveness = 42 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 42 dB

@Frequency 1.00e+9 Hz
42 dB

@Frequency 1.00e+9 Hz
1/8 thickness
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Shielding Effectiveness 42 dB

@Frequency 1.00e+10 Hz
42 dB

@Frequency 1.00e+10 Hz
P-Field
P & P Technology Monex Expanded Monel Foil
Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon..
Shielding Effectiveness 42 dB

@Frequency 10000 Hz
42 dB

@Frequency 10000 Hz
H-Field
P & P Technology VF Series Triple Mesh Dust Filter – Type VH-08
The VH-08 dust filter assemblies are constructed from three layers of corrugated aluminum mesh held in a ‘C’ section aluminum extruded frame. Please see standard profiles available in our catalogu..