Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | >= 46 dB @Frequency 14000 Hz |
>= 46 dB @Frequency 14000 Hz |
|
Parker Chomerics POLASTRIP® Metal EMI Gasket Description: POLASTRIP gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASTRIP gasketing, EMI shieldin.. |