Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 47 dB @Frequency 1.00e+8 Hz |
47 dB @Frequency 1.00e+8 Hz |
|
Parker Chomerics WIN-SHIELD™ Mesh 100 EMI Shielding Mesh Blackened copper plating. WIN-SHIELD Mesh 100 provides exceptional shielding performance and can be used as an optical product, to cover airflow openings, to wrap cable or other applications where .. |
|||
Shielding Effectiveness | 47 - 53 dB @Thickness 1.50 mm |
47 - 53 dB @Thickness 0.0591 in |
SABIC Method |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |