Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 52 dB @Frequency 10000 Hz |
52 dB @Frequency 10000 Hz |
H-Field |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Shielding Effectiveness | 52 dB @Frequency 1.00e+9 Hz |
52 dB @Frequency 1.00e+9 Hz |
E-Field |
P & P Technology VF Series Triple Mesh Dust Filter – Type VH-08 The VH-08 dust filter assemblies are constructed from three layers of corrugated aluminum mesh held in a ‘C’ section aluminum extruded frame. Please see standard profiles available in our catalogu.. |
|||
Shielding Effectiveness | 52 dB @Frequency 1.00e+9 Hz |
52 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Teckshield®-F 100 OPI 0.001" Diameter Wire, Allycarbonate EMI Shielding Window Description: Tecknit Allylcarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a lig.. |
|||
Shielding Effectiveness | 52 dB @Frequency 1.00e+10 Hz |
52 dB @Frequency 1.00e+10 Hz |
CHO-TP08 |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |