Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 56 dB @Frequency 1.00e+9 Hz |
56 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 56 dB @Frequency 1.00e+9 Hz |
56 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 56 dB @Frequency 1.00e+9 Hz |
56 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Teckshield®-F 50 OPI 0.001" Diameter Wire, Allycarbonate EMI Shielding Window Description: Tecknit Allycarbonate shielded windows are manufactured by casting a woven EMI shield mesh into a material that has optical properties similar to that of glass. The window offers a ligh.. |