Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 71 dB @Frequency 2.00e+8 Hz |
71 dB @Frequency 2.00e+8 Hz |
CHO-TP08 |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |