Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 85 dB @Thickness 1.60 mm, Frequency 1.00e+10 Hz |
85 dB @Thickness 0.0630 in, Frequency 1.00e+10 Hz |
MIL G83528 |
Rogers Corporation Bisco® EC-2130 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.063 inches and 0.125 inchesInformation provided by Rogers Corporation. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+9 Hz |
85 dB @Frequency 1.00e+9 Hz |
P-Field |
P & P Technology Monel-BS3075 (NA13) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | 85 dB @Frequency 2.00e+9 Hz |
85 dB @Frequency 2.00e+9 Hz |
Plane Wave; Mil-G-83528/MIL std 285 |
P & P Technology Nickel Graphite Loaded EPDM Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Infor.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+10 Hz |
85 dB @Frequency 1.00e+10 Hz |
Plane Wave; Mil-G-83528/MIL std 285 |
P & P Technology Nickel Graphite Loaded EPDM Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Infor.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+6 Hz |
85 dB @Frequency 1.00e+6 Hz |
H-Field |
P & P Technology Tinned Copper Steel (ASTM B520) Knitted Cored Shielding Mesh Product has a diameter of 0.11mm.Information provided by P & P Technology |
|||
Shielding Effectiveness | >= 85 dB @Frequency 1.00e+9 Hz |
>= 85 dB @Frequency 1.00e+9 Hz |
|
Parker Chomerics PORCUPINE METALASTIC® Gasketing Wire Mesh EMI Gasket Selection Guide Construction: Expanded Metal in ElastomerAvailable Forms: Sheets, Die-Cut GasketsStandard Metals Available in EMI Portion: Monel AluminumInformation provided by Chomerics |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+9 Hz |
85 dB @Frequency 1.00e+9 Hz |
ASTM D4935 |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+10 Hz |
85 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+10 Hz |
85 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+10 Hz |
85 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | >= 85 dB @Frequency 2.00e+9 Hz |
>= 85 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 85 dB @Frequency 1.00e+10 Hz |
>= 85 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 85 dB @Frequency 2.00e+9 Hz |
>= 85 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12 |
Parker Chomerics CHO-SEAL® 6435 Conductive Elastomer Description: Material of choice for high shielding effectiveness where NBC fluid resistance is needed; good performance in corrosive environments.Molded onlyRoHS CompliantInformation provided by Cho.. |
|||
Shielding Effectiveness | >= 85 dB @Frequency 1.00e+10 Hz |
>= 85 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12 |
Parker Chomerics CHO-SEAL® 6435 Conductive Elastomer Description: Material of choice for high shielding effectiveness where NBC fluid resistance is needed; good performance in corrosive environments.Molded onlyRoHS CompliantInformation provided by Cho.. |
|||
Shielding Effectiveness | >= 85 dB @Frequency 1.00e+10 Hz |
>= 85 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6452 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 85 dB @Frequency 1.00e+10 Hz |
>= 85 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+9 Hz |
85 dB @Frequency 1.00e+9 Hz |
|
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |
|||
Shielding Effectiveness | 85 dB @Frequency 1.00e+10 Hz |
85 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Shielding Effectiveness | 85 dB @Thickness 0.508 mm, Frequency 1.00e+10 Hz |
85 dB @Thickness 0.0200 in, Frequency 1.00e+10 Hz |
MIL G83528 |
Rogers Corporation Bisco® EC-2040 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.020 inches and 0.031 inchesInformation provided by Rogers Corporation. |