Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 98.5 dB @Frequency 4.00e+8 Hz |
98.5 dB @Frequency 4.00e+8 Hz |
P-Field, Electrical |
P & P Technology BS3075 NA13 Monel Wire Alloy 400L Wire Diameter 0.11mmInformation provided by P & P Technology |