Polymer Property : Shielding Effectiveness = 110 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 110 dB
110 dB
@ 100 MHz; Mil Std 285
Precision Polymer Engineering S70L Conductive Silicone Rubber
Tan coloured, Silicone Rubber, 66-75 °IRHD. Electrically conductive, Silver/Aluminum filled silicone rubber. Equivalent to Mil G 83528 Type D.Applications: Specially compounded to offer excellent ..
Shielding Effectiveness >= 110 dB
>= 110 dB
2 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 110 dB
>= 110 dB
10 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 110 dB
>= 110 dB
100 MHz (E Field); MIL-G-83528
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 110 dB
>= 110 dB
500 MHz (E Field); MIL-G-83528
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 110 dB
>= 110 dB
10 GHz (Plane Wave); MIL-G-83528
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Shielding Effectiveness >= 110 dB
>= 110 dB
500 MHz (E Field) - Base/Reinforced Material; MIL-G-83528
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Shielding Effectiveness >= 110 dB
>= 110 dB
100 MHz (E Field) - Base/Reinforced Material; MIL-G-83528
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..