Polymer Property : Shielding Effectiveness = 20 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 20 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
20 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc.
Shielding Effectiveness 20 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
20 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo..
Shielding Effectiveness 20 - 30 dB
20 - 30 dB
1000 MHz; ES7-83
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced