Polymer Property : Shielding Effectiveness = 36 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 36 dB

@Thickness 3.00 mm
36 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex KS003AI Acetal Copolymer (Europe-Africa-Middle East)
LNP* FARADEX* KS003AI is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include; EMI/RFI Shielding, Electrically Conductive.This data was supplied by SAB..