Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.0 kV/mm @Frequency 60.0 Hz |
279 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America FM 21386 Synthetic Fiber Reinforced Phenolic Novolac FM 21386 is a single stage phenolic molding compound reinforced with synthetic fiber in pellet form.Information provided by Sumitomo Bak North America, Inc. |