Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.4 kV/mm @Frequency 60.0 Hz |
290 kV/in @Frequency 60.0 Hz |
step-by-step, wet; ASTM D149 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |