Polymer Property : Dielectric Strength = 13.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 13.0 kV/mm

@Thickness 3.00 mm
330 kV/in

@Thickness 0.118 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS)
High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka..
Dielectric Strength 13.0 kV/mm

@Thickness 3.00 mm
330 kV/in

@Thickness 0.118 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS)
High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f..
Dielectric Strength 13.0 kV/mm

@Thickness 3.00 mm
330 kV/in

@Thickness 0.118 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS)
Easy flow, glossy, impact resistant.Applications: General purposeVarious technical parts, household appliances, hobby and office equipment, etc.Synthos was formerly known as Kaucuk. All information ..
Dielectric Strength 13.0 kV/mm

@Thickness 3.00 mm
330 kV/in

@Thickness 0.118 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 846 Acrylonitrile Butadiene Styrene (ABS)
High impact, medium flow, glossy, suitableApplications: General purpose, transport packaging, furniture, leisure time equipmentContainers, suitcases, profiles, ABS sheets, skis, helmets, garden equi..
Dielectric Strength 13.0 kV/mm

@Thickness 2.00 mm
330 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.5%); ASTM-D149
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..