Polymer Property : Dielectric Strength = 1450 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 57.0 kV/mm

@Thickness 0.500 mm
1450 kV/in

@Thickness 0.0197 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS)
Easy flow, glossy, impact resistant.Applications: General purposeVarious technical parts, household appliances, hobby and office equipment, etc.Synthos was formerly known as Kaucuk. All information ..