Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.4 kV/mm @Thickness 3.17 mm |
390 kV/in @Thickness 0.125 in |
in air; ASTM D149 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Dielectric Strength | 15.4 kV/mm @Thickness 3.17 mm |
390 kV/in @Thickness 0.125 in |
in oil; ASTM D149 |
Polymer Resources TP-GP1 Polybutylene Terephthalate, General Purpose, Flow Modified Polybutylene Terephthalate, General Purpose, Flow ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Dielectric Strength | >= 15.4 kV/mm @Temperature 121 °C, Time 10800 sec |
>= 392 kV/in @Temperature 250 °F, Time 3.00 hour |
0.0625 in. thickness; ASTM D149 |
Garlock BLUE-GARD® 3300 Compressed Aramid Fiber Gasketing, Neoprene Binder Aramid fiber, high-temperature fillers, and neoprene (CR) binder. Handles service conditions with refrigerants and various petroleum-based oils. Excellent SealabilityUnique blend of aramid fibers, f.. |
|||
Dielectric Strength | 15.4 kV/mm @Frequency 60.0 Hz |
391 kV/in @Frequency 60.0 Hz |
step-by-step, dry; ASTM D149 |
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc. |