Polymer Property : Dielectric Strength = 15.6 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength >= 15.6 kV/mm

@Temperature 121 °C,
Time 10800 sec
>= 396 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.0625 in. thickness; ASTM D149
Garlock BLUE-GARD® 3000 Compressed Aramid Fiber Gasketing, Nitrile Binder
Aramid fiber, high-temperature fillers, and nitrile (NBR) binder.Excellent SealabilityUnique blend of aramid fibers, fillers, and a NBR rubber binder provides improved torque retention and lowered e..
Dielectric Strength 15.6 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
396 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
DAM; Short Time; ASTM D149
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers