Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.3 kV/mm @Thickness 3.20 mm, Temperature 23.0 °C |
414 kV/in @Thickness 0.126 in, Temperature 73.4 °F |
DAM; Short Time; ASTM D149 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 16.3 kV/mm @Thickness 3.20 mm |
414 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM STM1500 PEI Copolymer Siloxane polyetherimide block copolymer. Wire and cable use. Strength and flexibility. |