Polymer Property : Dielectric Strength = 16.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 16.5 kV/mm

@Thickness 1.00 mm
419 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East)
LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo..
Dielectric Strength 16.5 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
419 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
500 V/s, in oil; Short Time; ASTM D149
DuPont Performance Polymers Rynite® 940 BK505 PET  (Unverified Data**)
Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers