Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.1 kV/mm @Thickness 3.20 mm |
434 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |