Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® FXS610SK ABS (Europe-Africa-Middle East) CYCOLAC FXS610SK is a multi purpose ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC FXS610SK is suitable for those applications that require sparkle c.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East) CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Lexan® 503R PC (Europe-Africa-Middle East) LEXAN 503R is a medium viscosity, 10% glass reinforced, UV-stabilized, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and exce.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
Conditioned; ASTM D149 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 2.00 mm |
457 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.00 mm |
457 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 3.00 mm |
457 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good electrical and mechanical properties by continuous use, even at high temperatures. Very good chemical resistance. Engineering and insulation material in electrical mac.. |
|||
Dielectric Strength | 18.0 kV/mm @Thickness 1.00 mm |
457 kV/in @Thickness 0.0394 in |
short time; IEC 60243-1 |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |